Burner Lance & Nose Ring

In cement factory, damage caused by abrasion and chemical attacks is considered one of the main factors in refractories destruction, especially in the kiln nose ring and burner tip. For this reason, the proper design and selection of refractories for these areas are important. the conditions of these areas are as follow:

•    Temperature 1300°c -1700°c
•    Thermal shock
•    Alkali & chemical attack
•    Corrosion & Abrasion
•    mechanical stress

Our solutions
High Alumina monolithic
specially containing Zirconia & SIC

 

 

 

Application area

Product

CCS (MPa)

Bulk Density (g/cm3)

CaO (%)

Burner

AT CAST MC 35 S 35

90 2.4 2.8-3.2

AT FLOW LA 55 SZ

75 2.8 <2.5

Nose ring

AT CAST LBT 85 S 5

80 2.8 1.5-2.5

AT CAST MC 35 S 35

90 2.4 2.8-3.2